Document Type : Original Reaearch Article
Authors
1
PhD candidate, Faculty of Materials and Metallurgical Engineering, Semnan University, Semnan, Iran.
2
Proffesor, Faculty of Materials and Metallurgical Engineering, Semnan University, Semnan, Iran.
3
Associate Proffesor, Faculty of Materials and Metallurgical Engineering, Semnan University, Semnan, Iran.
4
Associate Proffesor, Institute for Engineering in Medicine, Health, & Human Performance (EnMed), Batten College of Engineering and Technology, Old Dominion University, Norfolk, VA, 23529, USA.
10.30501/jamt.2026.597849.1373
Abstract
Background and Purpose: This study aimed to optimize both ink composition and extrusion-based three-dimensional (3D) printing parameters for the fabrication of polycaprolactone–nano-bioactive glass (PCL-BG) and polycaprolactone–nano-bioactive glass–Dorema ammoniacum (PCL-BG-DA) composite scaffolds.
Materials and Methods: PCL was dissolved in chloroform, and sol–gel-derived 45S5 nano-bioactive glass was incorporated into the solution. For DA-containing samples, Dorema ammoniacum powder was additionally added to the ink formulation. The effects of nano-bioactive glass content, the polycaprolactone-to-solvent ratio, print speed, and extrusion multiplier were evaluated using the Taguchi method. The fabricated scaffolds were characterized in terms of printability, microstructure, and compressive properties.
Results: The results demonstrated that the nano-bioactive glass content of the ink was the most influential factor affecting printability, compared with print speed and extrusion multiplier. Optimal printing conditions were achieved using a polymer-to-powder ratio of 3:1, a polymer-to-solvent ratio of 1:2, a retraction value of 1.65, an extrusion multiplier of 0.0120, and a print speed of 5. Under these conditions, scaffolds with acceptable printing quality, high reproducibility, and considerable flexibility in both shape and size were successfully fabricated. Scanning electron microscopy (SEM) images confirmed the presence of a porous and interconnected structure. The incorporation of DA reduced the compressive modulus from 53.737 MPa to 38.527 MPa.
Conclusion: The simultaneous optimization of ink composition and printing parameters enabled the successful fabrication of PCL-BG and PCL-BG-DA composite scaffolds. Nano-bioactive glass content was identified as the primary factor governing printability, while the addition of DA preserved satisfactory printability and reduced scaffold stiffness.