Ti-Al-Al2O3 composite is produced from Al and TiO2 particles by a mechanochemical method. The starting powders were first activated by high-energy milling which reduced the grain sizes down to nanometric scale. Then, the milled powders were annealed at 600◦C for 5hr in order to decrease the activation energy for the formation of Al2O3 and Ti-Al binary compounds. Results indicated the formation of some TiAl and Ti3Al compounds. However, to complete this process, it was necessary to perform a subsequent heat treatment of the previously anneald samples at 1200, 1300 and 1400◦C.
Yazdani Rad,R. and Motiei Mehr,M. (2013). Parameters Affecting the Mechanochemical Synthesis of
Ti-Al-Al2O3 Composites from Al and TiO2 powders. Journal of Advanced Materials and Technologies, 1(2), 69-78. doi: 10.30501/jamt.2010.70143
MLA
Yazdani Rad,R. , and Motiei Mehr,M. . "Parameters Affecting the Mechanochemical Synthesis of
Ti-Al-Al2O3 Composites from Al and TiO2 powders", Journal of Advanced Materials and Technologies, 1, 2, 2013, 69-78. doi: 10.30501/jamt.2010.70143
HARVARD
Yazdani Rad R., Motiei Mehr M. (2013). 'Parameters Affecting the Mechanochemical Synthesis of
Ti-Al-Al2O3 Composites from Al and TiO2 powders', Journal of Advanced Materials and Technologies, 1(2), pp. 69-78. doi: 10.30501/jamt.2010.70143
CHICAGO
R. Yazdani Rad and M. Motiei Mehr, "Parameters Affecting the Mechanochemical Synthesis of
Ti-Al-Al2O3 Composites from Al and TiO2 powders," Journal of Advanced Materials and Technologies, 1 2 (2013): 69-78, doi: 10.30501/jamt.2010.70143
VANCOUVER
Yazdani Rad R., Motiei Mehr M. Parameters Affecting the Mechanochemical Synthesis of
Ti-Al-Al2O3 Composites from Al and TiO2 powders. J. Adv. Mater. Technol., 2013; 1(2): 69-78. doi: 10.30501/jamt.2010.70143